The highest lithium leaching efficiency achieved 90.3% when 15% ferric chloride was used at 90 °C, for 180 min, from clay calcined at 700 °C. In addition to the high leaching efficiencies, more important benefits of using ferric salt are that the leaching process is green and that weakly-acidic residues are discharged.